Material Notes:
HexPly® 108 is a high temperature resistant epoxy resin system developed for the fabrication of primary aircraft and space structures. 108 has excellent hot wet properties and exhibits low viscosity.Features: High temperature performance, High flow matrix, Low tack, Good hot wet properties up to 145°C
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
Cured resin density
Mechanical Properties Metric English Comments
Tensile Strength, Yield 59.0 MPa
8560 psi
ISO R527
Elongation at Yield 1.7 %
1.7 %
ISO R527
Tensile Modulus 3.54 GPa
513 ksi
ISO R527
Flexural Yield Strength 94.0 MPa
13600 psi
ISO 178
Flexural Modulus 2.40 GPa
348 ksi
ISO 178
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 190 - 210 °C
374 - 410 °F
DMA
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F