Material Notes:
HexPly® 914 is a highly successful modified epoxy matrix which is used extensively in high temperature resistant primary aircraft structures. The controlled melt viscosity and excellent matrix rheology of 914 permits a wide range of processing conditions for high quality components.Features: High melt viscosity giving easy processing characteristics, Tolerant to a wide variation of processing conditions, Latitude for low to high pressure laminating or moulding processes, Medium tack level giving excellent drape characteristics, Good shelf life
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
Cured
Mechanical Properties Metric English Comments
Tensile Strength, Yield 47.7 MPa
6920 psi
ISO R527 type 1
Elongation at Yield 1.5 %
1.5 %
ISO R527 type 1
Tensile Modulus 3.90 GPa
566 ksi
ISO R527 type 1
Compressive Yield Strength 180 MPa
26100 psi
ISO 604
Poissons Ratio 0.41
0.41
ISO R527 type 1
Fracture Toughness 0.700 MPa-m½
0.637 ksi-in½
Shear Modulus 1.40 GPa
203 ksi
ISO R527 type 1
Toughness 103 J
76.0 ft-lb
Per square meter
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 190 °C
374 °F
DMTA
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Tack Life (days) 60