Material Notes:
HexPly® 924 is a controlled flow epoxy matrix developed for the fabrication of high temperature resistant primary structures. When cured, HexPly® 924 becomes a tough composite with high impact resistance and damage tolerance. It is particularly suitable for aircraft primary structures and elevated temperature applications such as performance cars.HexPly® 924 is best suited to autoclave or press cure to obtain optimum mechanical performance from the cured composite.Information provided by HexCel
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
Cured
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.0 MPa
9430 psi
ISO R527 type 1
Elongation at Yield 2.4 %
2.4 %
ISO R527 type 1
13 %
13 %
Compression Strain; ISO 604
Tensile Modulus 3.80 GPa
551 ksi
ISO R527 type 1
Flexural Yield Strength 120 MPa
17400 psi
ISO 178
Flexural Modulus 3.12 GPa
453 ksi
ISO 178
Compressive Yield Strength 175 MPa
25400 psi
ISO 604
Poissons Ratio 0.41
0.41
ISO R527 type 1
Fracture Toughness 0.830 MPa-m½
0.755 ksi-in½
Shear Modulus 1.34 GPa
194 ksi
ISO R527 type 1
Toughness 150 J
111 ft-lb
Per square meter
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 190 °C
374 °F
DMTA
Shrinkage 1.6 %
1.6 %
Processing Properties Metric English Comments
Shelf Life >= 12.0 Month

@Temperature -18.0 °C
>= 12.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Tack Life (days) 21
Users viewing this material also viewed the following: