Hexcel® HexPly® 954-3 Curing Cyanate Resin, YSH-60A Fiber

Category Polymer , Thermoset , Epoxy
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® 954-3 Curing Cyanate Resin, YSH-60A Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.0 MPa

@Temperature 23.0 °C
4640 psi

@Temperature 73.4 °F
90°
2289 MPa

@Temperature 23.0 °C
332000 psi

@Temperature 73.4 °F
Tensile Modulus 38.0 GPa

@Temperature 23.0 °C
5510 ksi

@Temperature 73.4 °F
90°
391 GPa

@Temperature 23.0 °C
56700 ksi

@Temperature 73.4 °F
Compressive Yield Strength 476 MPa

@Temperature 23.0 °C
69000 psi

@Temperature 73.4 °F
Compressive Modulus 335 GPa

@Temperature 23.0 °C
48600 ksi

@Temperature 73.4 °F
Shear Strength 65.0 MPa

@Temperature 22.0 °C
9430 psi

@Temperature 71.6 °F