Hexcel® HexPly® 954-3A Curing Cyanate Resin, M60J Fiber

Category Polymer , Thermoset , Epoxy
Manufacturer Hexcel
Trade Name HexPly®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® 954-3A Curing Cyanate Resin, M60J Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2120 MPa

@Temperature 23.0 °C
307000 psi

@Temperature 73.4 °F
Tensile Modulus 391 GPa

@Temperature 23.0 °C
56700 ksi

@Temperature 73.4 °F
Flexural Yield Strength 858 MPa

@Temperature 23.0 °C
124000 psi

@Temperature 73.4 °F
Flexural Modulus 274 GPa

@Temperature 23.0 °C
39700 ksi

@Temperature 73.4 °F
Compressive Yield Strength 827 MPa

@Temperature 23.0 °C
120000 psi

@Temperature 73.4 °F
Compressive Modulus 333 GPa

@Temperature 23.0 °C
48300 ksi

@Temperature 73.4 °F
Shear Modulus 3.70 GPa
537 ksi
In-Plane
Shear Strength 45.0 MPa
6530 psi
In-Plane