Material Notes:
Information provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 36.5 MPa

@Temperature 23.0 °C
5290 psi

@Temperature 73.4 °F
Flatwise, 0°
72.0 MPa

@Temperature 23.0 °C
10400 psi

@Temperature 73.4 °F
90°
2365 MPa

@Temperature 23.0 °C
343000 psi

@Temperature 73.4 °F
Tensile Modulus 7.60 GPa

@Temperature 23.0 °C
1100 ksi

@Temperature 73.4 °F
90°
196 GPa

@Temperature 23.0 °C
28400 ksi

@Temperature 73.4 °F
Compressive Yield Strength 2000 MPa

@Temperature 23.0 °C
290000 psi

@Temperature 73.4 °F
Compressive Modulus 222 GPa

@Temperature 23.0 °C
32200 ksi

@Temperature 73.4 °F
Shear Modulus 4.60 GPa

@Temperature 23.0 °C
667 ksi

@Temperature 73.4 °F
Shear Strength 99.0 MPa

@Temperature 22.0 °C
14400 psi

@Temperature 71.6 °F
0°, IL
127 MPa

@Temperature 23.0 °C
18400 psi

@Temperature 73.4 °F
Users viewing this material also viewed the following: