Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, High Modulus 12k carbon UD tape 110 g/m2

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, High Modulus 12k carbon UD tape 110 g/m2.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1750 MPa
254000 psi
Tensile Modulus 210 GPa
30500 ksi
Flexural Yield Strength 1300 MPa
189000 psi
Flexural Modulus 185 GPa
26800 ksi
Compressive Yield Strength 1100 MPa
160000 psi
Shear Strength 80.0 MPa
11600 psi
0°, Short Beam
Processing Properties Metric English Comments
Shelf Life 14.0 Month

@Temperature -18.0 °C
14.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Fiber Volume (%) 60
Tack Life (days) 30