Material Notes:
AS4C 150 24" EH04 35%; Normalized to 55% fiber volume; 75°F, dryInformation provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2320 MPa
336000 psi
Tensile Modulus 125 GPa
18100 ksi
Flexural Yield Strength 1320 MPa
191000 psi
Flexural Modulus 117 GPa
16900 ksi
Compressive Yield Strength 1500 MPa
218000 psi
Compressive Modulus 117 GPa
16900 ksi
Shear Strength 84.1 MPa
12200 psi
Short Beam