IM4 120 24" EH04 31%; Normalized to 55% fiber volume; 75°F, dryInformation provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2230 MPa
323000 psi
Tensile Modulus 145 GPa
21100 ksi
Flexural Yield Strength 1400 MPa
203000 psi
Flexural Modulus 132 GPa
19200 ksi
Compressive Yield Strength 1530 MPa
222000 psi
Compressive Modulus 138 GPa
20000 ksi
Shear Strength 85.5 MPa
12400 psi
Short Beam