Hexcel® HexPly® EH04 Epoxy Resin System, MS40 Fiber

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® EH04 Epoxy Resin System, MS40 Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MS40 120 24" EF04 31%; Normalized to 55% fiber volume; 75°F, dryInformation provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2560 MPa
372000 psi
Tensile Modulus 184 GPa
26700 ksi
Flexural Yield Strength 1330 MPa
193000 psi
Flexural Modulus 165 GPa
24000 ksi
Compressive Yield Strength 1610 MPa
233000 psi
Compressive Modulus 168 GPa
24300 ksi
Shear Strength 84.1 MPa
12200 psi
Short Beam