Hexcel® HexPly® ES 84 120°C Curing Epoxy Matrix, Aramid Balanced fabric 175 g/m2

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® ES 84 120°C Curing Epoxy Matrix, Aramid Balanced fabric 175 g/m2.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 600 MPa
87000 psi
Tensile Modulus 32.0 GPa
4640 ksi
Flexural Yield Strength 380 MPa
55100 psi
Flexural Modulus 21.0 GPa
3050 ksi
Compressive Yield Strength 240 MPa
34800 psi
Shear Strength 35.0 MPa
5080 psi
0°, Short Beam
Processing Properties Metric English Comments
Shelf Life 14.0 Month

@Temperature -18.0 °C
14.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Fiber Volume (%) 50
Tack Life (days) 30