Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HexPly® ES70 is a structural epoxy resin particularly well adapted to low pressure molding processes. This system is versatile and allows a polymerization from 100°C (212°F) up to 150°C (302°F). HexPly® ES70 can be used for industrial, sports and leisure application.HexPly® ES70 prepreg is available in fabrics reinforcement.Information provided by HexCel
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
Cured resin
Mechanical Properties Metric English Comments
Tensile Strength, Yield 70.0 MPa
10200 psi
ISO R527
Elongation at Yield 2.7 %
2.7 %
ISO R527
Tensile Modulus 2.90 GPa
421 ksi
ISO R527
Poissons Ratio 0.35
0.35
Shear Modulus 1.07 GPa
155 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 75.1 µm/m-°C
41.7 µin/in-°F
ASTM D696.79
Glass Transition Temp, Tg 100 °C
212 °F
DMA
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Tack Life (days) 30