Material Notes:
HexPly® ES/EH 84 matrix is a structural epoxy resin for tubular parts designed for low pressure curing in the manufacture of sports goods and for industrial applications. It is ideal for the following processes: shrink wrap tape, vacuum bag, press and autoclave manufacturing methods.HexPly® ES 84 is supplied with fabric reinforcement. HexPly® EH 84 is a UD tape.Features: Maximum service temperature 85°C ( 185°F), Low exotherm, Low pressure moulding, Good surface aspect, Low viscosity, Low density, Versatile cure process 100-140°C (212- 285°F), Good flexibility
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Cured resin
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
ISO R527
Elongation at Yield 2.1 %
2.1 %
ISO R527
Tensile Modulus 3.00 GPa
435 ksi
ISO R527
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 95.0 °C
203 °F
DMA
Processing Properties Metric English Comments
Shelf Life 14.0 Month

@Temperature -18.0 °C
14.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Tack Life (days) 30