Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® HexPly® F155 Epoxy Resin, K120 Kevlar Fabric

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® F155 Epoxy Resin, K120 Kevlar Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fiber: Kev. 49 195Information provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.137 MPa

@Temperature 71.0 °C
600.0 psi

@Temperature 160 °F
Flatwise TS
5.516 MPa

@Temperature 24.0 °C
800.0 psi

@Temperature 75.2 °F
Flatwise TS
400 MPa

@Temperature 71.0 °C
58000 psi

@Temperature 160 °F
427 MPa

@Temperature 24.0 °C
61900 psi

@Temperature 75.2 °F
Tensile Modulus 25.0 GPa

@Temperature 71.0 °C
3630 ksi

@Temperature 160 °F
26.7 GPa

@Temperature 24.0 °C
3870 ksi

@Temperature 75.2 °F
Compressive Yield Strength 165 MPa

@Temperature 71.0 °C
23900 psi

@Temperature 160 °F
221 MPa

@Temperature 24.0 °C
32100 psi

@Temperature 75.2 °F
Compressive Modulus 21.0 GPa

@Temperature 71.0 °C
3050 ksi

@Temperature 160 °F
26.9 GPa

@Temperature 24.0 °C
3900 ksi

@Temperature 75.2 °F
Descriptive Properties Value Comments
Cured Thickness per Ply (cm) 0.011
Laminate
Dry Resin Content (%) 54-60
Prepreg
Fiber Volume (%) 42
Laminate
Flow (%) 14-26