Material Notes:
Information provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.413 MPa

@Temperature 71.0 °C
640.1 psi

@Temperature 160 °F
Flatwise TS
5.164 MPa

@Temperature 24.0 °C
749.0 psi

@Temperature 75.2 °F
Flatwise TS
547 MPa

@Temperature 71.0 °C
79300 psi

@Temperature 160 °F
571 MPa

@Temperature 24.0 °C
82800 psi

@Temperature 75.2 °F
Tensile Modulus 26.9 GPa

@Temperature 71.0 °C
3900 ksi

@Temperature 160 °F
30.3 GPa

@Temperature 24.0 °C
4390 ksi

@Temperature 75.2 °F
Compressive Yield Strength 195 MPa

@Temperature 71.0 °C
28300 psi

@Temperature 160 °F
261 MPa

@Temperature 24.0 °C
37900 psi

@Temperature 75.2 °F
Compressive Modulus 23.4 GPa

@Temperature 24.0 °C
3390 ksi

@Temperature 75.2 °F
23.4 GPa

@Temperature 71.0 °C
3390 ksi

@Temperature 160 °F
Descriptive Properties Value Comments
Cured Thickness per Ply (cm) 0.0025
Laminate
Dry Resin Content (%) 49-55
Prepreg
Fiber Volume (%) 46
Laminate
Flow (%) 14-26