Hexcel® HexPly® M12 135°C Curing Epoxy Matrix

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® M12 135°C Curing Epoxy Matrix.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HexPly® M12 is a good performance, self extinguishing, tough epoxy matrix for use in helicopter blades. It exhibits good fatigue life and hot/wet performances up to 100ºC. HexPly® M12 is supplied with R-glass UD tape, glass and carbon woven fibers. HexPly® M12 was developed for low exotherm curing, so parts with thickness above 10 cm can be cured directly to 135ºC without any exothermal risks.Information provided by HexCel
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 64.0 MPa
9280 psi
Elongation at Yield 1.26 %
1.26 %
Tensile Modulus 5.10 GPa
740 ksi
Poissons Ratio 0.40
0.40
Shear Modulus 1.82 GPa
264 ksi
Calculated
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 128 °C
262 °F
Wet
Processing Properties Metric English Comments
Shelf Life 14.0 Month

@Temperature -18.0 °C
14.0 Month

@Temperature -0.400 °F