Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® HexPly® M14 248°F (120°C) Curing Epoxy Matrix

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® M14 248°F (120°C) Curing Epoxy Matrix.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HexPly® M14 is a modified epoxy resin which provides good adhesion to honeycomb and foam cores. Its self-extinguishing characteristics meet the fire, smoke, and toxicity requirements of aerospace and railway specifications. HexPly® M14 can be used for very large industrial components subjected to severe environmental conditions.Information provided by HexCel
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
Cured resin
Mechanical Properties Metric English Comments
Tensile Strength, Yield 70.0 MPa
10200 psi
ISO R527
Elongation at Yield 2.9 %
2.9 %
ISO R527
Tensile Modulus 3.20 GPa
464 ksi
ISO R527
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 110 - 130 °C
230 - 266 °F
DMA
Processing Properties Metric English Comments
Shelf Life 1.00 Month

@Temperature 23.0 °C
1.00 Month

@Temperature 73.4 °F
12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F
Guaranteed
Copyright © lookpolymers.com All Rights Reserved