Hexcel® HexPly® M26/M26T 120°C (250°F) Curing Epoxy Matrix

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® M26/M26T 120°C (250°F) Curing Epoxy Matrix.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HexPly® M26 is an advance modified epoxy resin developed for aerospace and industrial markets. Its controlled flow, high peel strength on honeycomb cores and excellent fire behavior give it a cost saving potential for interior and secondary sandwich structures. Combined with HexPly® M25 glass phenolic prepregs, it is qualified to Airbus specifications.Two grades available: M26, reduced tack grade, for flat panels applications; M26T, improved tack grade, for other sandwich structures.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
Cured
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 90.0 °C
194 °F
105 °C
221 °F
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Tack Life (days) 30