Hexcel® HexPly® M34 75°C (167°F) Curing Epoxy Matrix

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® M34 75°C (167°F) Curing Epoxy Matrix.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HexPly® M34 is an epoxy system, specifically developed for low temperature curing of large structural components, particularly in industrial markets. HexPly® M34 is a self-extinguishing system, providing excellent fire-resistant properties, and meeting the German and French rail qualifications DIN 5510, S3-SR2-ST2 and NF F 16-101 (M2, F1). HexPly® M34 prepreg is ideal for manufacturing sandwich structures, providing excellent adhesion to PVC foam cores. HexPly® M34 exhibits a good shelf life at room temperature for a low temperature curing system.Information provided by HexCel
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
Mechanical Properties Metric English Comments
Flexural Yield Strength 120 MPa
17400 psi
Flexural Modulus 3.80 GPa
551 ksi
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 80.0 °C
176 °F
DMA
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F