Material Notes:
Fiber: T300 3K, 285 g/m2Information provided by HexCel
Physical Properties Metric English Comments
Density 1.51 g/cc
0.0546 lb/in³
Nominal Laminate Density
Mechanical Properties Metric English Comments
Compressive Yield Strength 771 MPa

@Temperature 23.0 °C
112000 psi

@Temperature 73.4 °F
prEN2580 Type A
Shear Strength 35.0 MPa

@Temperature 140 °C
5080 psi

@Temperature 284 °F
ILSS; prEN2563
49.0 MPa

@Temperature 120 °C
7110 psi

@Temperature 248 °F
ILSS; prEN2563
55.0 MPa

@Temperature 100 °C
7980 psi

@Temperature 212 °F
ILSS; prEN2563
59.0 MPa

@Temperature 23.0 °C
8560 psi

@Temperature 73.4 °F
ILSS; prEN2563
61.0 MPa

@Temperature 80.0 °C
8850 psi

@Temperature 176 °F
ILSS; prEN2563
Processing Properties Metric English Comments
Shelf Life >= 12.0 Month

@Temperature -18.0 °C
>= 12.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Cured Thickness per Ply (cm) 0.0314
Fiber Volume (%) 51.6