Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, 3K High Strength Carbon

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, 3K High Strength Carbon.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fiber Designation: C280T4; Twill 4x4Information provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 882 MPa

@Temperature 23.0 °C
128000 psi

@Temperature 73.4 °F
0°, Conditioning: 23°C; ASTM D3039
Tensile Modulus 56.0 GPa

@Temperature 23.0 °C
8120 ksi

@Temperature 73.4 °F
0°, Conditioning: 23°C; ASTM D3039
Flexural Yield Strength 515 MPa

@Temperature 90.0 °C
74700 psi

@Temperature 194 °F
0°, Conditioning: 23°C; ASTM D790
818 MPa

@Temperature 23.0 °C
119000 psi

@Temperature 73.4 °F
0°, Conditioning: 23°C; ASTM D790
Compressive Yield Strength 422 MPa

@Temperature 90.0 °C
61200 psi

@Temperature 194 °F
0°, Conditioning: 23°C; ASTM D965
514 MPa

@Temperature 23.0 °C
74500 psi

@Temperature 73.4 °F
0°, Conditioning: 23°C; ASTM D965
Shear Strength 36.0 MPa

@Temperature 90.0 °C
5220 psi

@Temperature 194 °F
0°, Interlaminar, Conditioning: 23°C; ASTM D2344
66.0 MPa

@Temperature 23.0 °C
9570 psi

@Temperature 73.4 °F
0°, Interlaminar, Conditioning: 23°C; ASTM D2344
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Dry Resin Content (%) 42
Fiber Volume (%) 49.5