Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HexPly® M56 is a high performance epoxy matrix developed for out-of-autoclave curing of secondary aircraft structures.Features: Matrix specifically formulated for vacuum pressure only cure, Product formats designed to optimise fibre volume, Low density matrix can contribute to increased weight savings, Available as carbon UD tape, woven carbon, woven glass and metallic meshes, 30 days room temperature tack life, Excellent drape and tack, Suitable for ATL and AFP processing
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F