Material Notes:
HexTow™ AS7 carbon fiber is a continuous, high strength, high strain, PAN based fiber available, in a 12,000 (12K) filament count tow. This fiber has been surface treated and can be sized to improve its interlaminar shear properties, handling characteristics, and structural properties. Suggested for use in prepregging, weaving, and filament winding.Information provided by Hexcel
Physical Properties Metric English Comments
Density 1.79 g/cc
0.0647 lb/in³
Filament Diameter 6.9 µm
6.9 µm
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2415 MPa
350300 psi
Typical epoxy composite property
4830 MPa
701000 psi
Typical fiber property
Elongation at Break 1.8 %
1.8 %
Calculated from tow test data
Tensile Modulus 152 GPa
22000 ksi
Typical epoxy composite property
241 GPa
35000 ksi
Typical fiber property; Chord 6000-1000
Flexural Modulus 128 GPa
18600 ksi
Typical epoxy composite property
Shear Strength 124 MPa
18000 psi
Typical epoxy composite property; short-beam
Component Elements Properties Metric English Comments
Carbon, C 94 %
94 %
Descriptive Properties Value Comments
Approximate Yield (m/g) 1.25
12K
Fiber Volume (%) 62
Tow Cross-Sectional Area (mm2) 0.45
12K
Weight/Length (g/m) 0.8
12K