Hexcel® HexTow™ IM9 Carbon Fiber

Category Carbon , Carbon Fiber
Manufacturer Hexcel
Trade Name HexTow™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexTow™ IM9 Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HexTow™ IM9 carbon fiber is a continuous, ultrahigh performance, intermediate modulus, PAN based fiber available in 12,000 (12K) filament count tows. The fiber has been surface treated and can be sized to improve its interlaminar shear properties, handling characteristics, and structural properties. HexTow™ IM9 fiber has shear properties equivalent to those of standard AS type fibers. It is suggested for use in weaving, braiding, prepregging and filament.The unique properties of HexTow™ IM9 fiber, such as ultrahigh tensile strength and good compressive strength, as well as good shear strength, allow structural designers to achieve both higher safety margins for both stiffness and strength critical applications.Information provided by Hexcel
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
Filament Diameter 4.4 µm
4.4 µm
Mechanical Properties Metric English Comments
Tensile Strength, Yield 3222 MPa
467300 psi
Typical epoxy composite property
6140 MPa
891000 psi
Typical fiber property
Elongation at Break 1.9 %
1.9 %
Calculated from tow test data
Tensile Modulus 176 GPa
25500 ksi
Typical epoxy composite property
304 GPa
44100 ksi
Typical fiber property; Chord 6000-1000
Flexural Modulus 152 GPa
22000 ksi
Typical epoxy composite property
Shear Strength 124 MPa
18000 psi
Typical epoxy composite property; short-beam
Component Elements Properties Metric English Comments
Carbon, C 94 %
94 %
Descriptive Properties Value Comments
Approximate Yield (m/g) 2.99
12K
Fiber Volume (%) 62
Tow Cross-Sectional Area (mm2) 0.19
12K
Weight/Length (g/m) 0.335
12K
Users viewing this material also viewed the following: