Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® HexTow™ PV42/850 Carbon Fiber

Category Carbon , Carbon Fiber
Manufacturer Hexcel
Trade Name HexTow™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexTow™ PV42/850 Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HexTow™ PV42/850 (HS-CP-3300) carbon fiber is a continuous, high performance, intermediate modulus, PAN based fiber available in 12,000 (12K) filament count tows. This fiber has been designed for applications that require high composite tensile strength. The fiber can be sized to improve its handling characteristics. HexTow™ PV42/850 (HS-CP-3300) fiber is suggested for use in filament winding for pressure vessels and other similar applications.The unique properties of HexTow™ PV42/850 (HS-CP-3300) fiber allow structural designers to achieve higher safety margins for strength critical applications.Information provided by Hexcel
Physical Properties Metric English Comments
Density 1.79 g/cc
0.0647 lb/in³
Filament Diameter 5.1 µm
5.1 µm
Mechanical Properties Metric English Comments
Tensile Strength, Yield 3378 MPa
489900 psi
Typical epoxy composite property
5810 MPa
843000 psi
Typical fiber property
Elongation at Break 1.9 %
1.9 %
Calculated from tow test data
Tensile Modulus 178 GPa
25800 ksi
Typical epoxy composite property
292 GPa
42400 ksi
Typical fiber property; Chord 6000-1000
Flexural Modulus 148 GPa
21500 ksi
Typical epoxy composite property
Shear Strength 93.0 MPa
13500 psi
Typical epoxy composite property; short-beam
Component Elements Properties Metric English Comments
Carbon, C 94 %
94 %
Descriptive Properties Value Comments
Approximate Yield (m/g) 2.24
Fiber Volume (%) 62
Tow Cross-Sectional Area (mm2) 0.25
Weight/Length (g/m) 0.446
12K
Users viewing this material also viewed the following: