Hexcel® HexWeb® CR-PAA™ 1/4-5052-0.004 Phosphoric Acid Anodized Aluminum Honeycomb

Category Metal , Metal Foam, Mesh, or Honeycomb , Nonferrous Metal , Aluminum Alloy , 5000 Series Aluminum Alloy
Manufacturer Hexcel
Trade Name HexWeb®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexWeb® CR-PAA™ 1/4-5052-0.004 Phosphoric Acid Anodized Aluminum Honeycomb.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the face sheets that carry bending loads and the honeycomb that carries the shear loads. The adhesive is the interface between the facing and the core in the same way that the oxide on the aluminum and the primer that has been applied to it is the interface between the honeycomb substrate material and the bonding adhesive. This interface is critical to the performance of honeycomb bonded assemblies.HexWeb® CR-PAA™ is designed for aircraft structures that are exposed to demanding environmental conditions. HexWeb® CR-PAA™ outperforms standard MIL-C-7438 core in salt spray and HexWeb® crack propagation tests.
Physical Properties Metric English Comments
Density 0.127 g/cc
0.00457 lb/in³
Nominal
Mechanical Properties Metric English Comments
Compressive Yield Strength >= 6.69 MPa
>= 970 psi
Bare, min
>= 7.24 MPa
>= 1050 psi
Stabilized, min
9.79 MPa
1420 psi
Bare, typ
10.3 MPa
1490 psi
Stabilized, typ
Compressive Modulus 2.34 GPa
340 ksi
Stabilized, typ
Shear Modulus 0.364 GPa
52.8 ksi
Plate Shear, W Direction, typ
0.896 GPa
130 ksi
Plate Shear, L Direction, typ
Shear Strength >= 2.69 MPa
>= 390 psi
Plate Shear, W Direction, min
3.03 MPa
440 psi
Plate Shear, W Direction, typ
>= 4.48 MPa
>= 650 psi
Plate Shear, L Direction, min
4.83 MPa
700 psi
Plate Shear, L Direction, typ