Hexcel® Redux® 112 Surface Pretreatment Protection Solution

Category Fluid , Polymer , Adhesive
Manufacturer Hexcel
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® Redux® 112 Surface Pretreatment Protection Solution.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Redux 100 series is a range of resin solutions used for protecting light alloy surfaces that have been pretreated for bonding but must be stored temporarily before bonding is completed.A thin coating of solution applied to freshly pretreated and dried surfaces loses solvent rapidly at room temperature, sealing the surfaces from the atmosphere and protecting them from loss of pretreatment quality for storage periods of up to 2 months.The Redux 100 series is intended for use with associated Redux film adhesives. When used with the corresponding Redux adhesive, the surface pretreatment protection does not need to be removed or cured prior to bonding.Cleaning solution: Acetone or Methyl ethyl ketone (MEK)
Physical Properties Metric English Comments
Storage Temperature 4.44 - 26.7 °C
40.0 - 80.0 °F
Processing Properties Metric English Comments
Drying Temperature 71.1 °C
160 °F
Dry Time >= 0.333 hour
>= 0.333 hour
Shelf Life 24.0 Month
24.0 Month
At storage temperature
Descriptive Properties Value Comments
Color Yellow
Corresponding Adhesive Redux 312, 335, 382H, 609