Hexcel® Redux® 308A-NA Modified epoxy film adhesive

Category Polymer , Adhesive , Film , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Hexcel
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® Redux® 308A-NA Modified epoxy film adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Redux 308A-NA is a high-strength, flow-controlled film adhesive with flexible cure schedules at 300°F or 350°F. Redux 308A-NA contains glass beads that give good flow control. It is suitable for metal to metal and structural sandwich bonding applications where operating temperatures of up to 250°F may be experienced.Features: Flexible curing schedule: 300°F or 350°F; 300°F cure gives excellent peel performance; 350°F cure gives excellent lap shear performance; Good structural performance to 250°F; Excellent environmental resistance; Glass beads ensure glue line thickness control; Low volatile content (solventless process).Applications: Metal to metal bonding; Structural sandwich constructions.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 8.27 MPa

@Temperature 21.1 °C
1200 psi

@Temperature 70.0 °F
Flatwise Tensile
Shear Strength 20.0 MPa

@Temperature 121 °C
2900 psi

@Temperature 250 °F
Lap Shear
40.0 MPa

@Temperature 71.1 °C
5800 psi

@Temperature 160 °F
Lap Shear
46.2 MPa

@Temperature 21.1 °C
6700 psi

@Temperature 70.0 °F
Lap Shear
Peel Strength 10.2 kN/m

@Temperature 21.1 °C
58.0 pli

@Temperature 70.0 °F
Bell Peel
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -17.8 °C
12.0 Month

@Temperature 0.000 °F
Descriptive Properties Value Comments
Areal Weight (psf) 0.06
Climbing Drum Peel (in-lb/3in) 75
70°F
Roll Width (in) 21
Standard Roll (ft2) 430