Material Notes:
Used in mechanical and electrical applications. Extremely high mechanical strength at moderate temperature. Very good electrical properties under high humidity.Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.70 - 1.90 g/cc
1.70 - 1.90 g/cc
IEC 1212-2 8.1
Mechanical Properties Metric English Comments
Tensile Strength >= 250 MPa
>= 36300 psi
IEC 1212-2 5.7
Flexural Strength >= 320 MPa
>= 46400 psi
Perpendicular to laminations; IEC 1212-2 5.1
Flexural Modulus >= 15.0 GPa
>= 2180 ksi
IEC 1212-2 5.2
Compressive Strength >= 350 MPa
>= 50800 psi
Perpendicular to laminations; IEC 1212-2 5.3
Shear Strength >= 20.0 MPa
>= 2900 psi
Parallel to laminations; IEC 1212-2 5.6
Izod Impact, Unnotched (ISO) >= 54.0 kJ/m²
>= 25.7 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.3
Charpy Impact Unnotched >= 5.00 J/cm²
>= 23.8 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.2
Electrical Properties Metric English Comments
Insulation Resistance >= 5.00e+9 ohm
>= 5.00e+9 ohm
After immersion in water; IEC 1212-2 6.3
Dielectric Constant <= 5.5

@Frequency 48.0 - 62.0 Hz
<= 5.5

@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
<= 5.5

@Frequency 1.00e+6 Hz
<= 5.5

@Frequency 1.00e+6 Hz
IEC 1212-2 6.2
Dielectric Breakdown >= 35000 V

@Temperature 90.0 °C
>= 35000 V

@Temperature 194 °F
In oil, parallel to laminations; IEC 1212-2 6.2
Dissipation Factor <= 0.050

@Frequency 48.0 - 62.0 Hz
<= 0.050

@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
<= 0.050

@Frequency 1.00e+6 Hz
<= 0.050

@Frequency 1.00e+6 Hz
IEC 1212-2 6.2
Comparative Tracking Index >= 200 V
>= 200 V
IEC 1212-2 6.4
Descriptive Properties Value Comments
Thermal Endurance 130 T.I.
IEC 1212-2 7.1
Water Absorption < 40 mg
IEC 1212-2 8.2; Test piece 50 x 50 x 10 mm