Material Notes:
Used in electrical and mechanical applications. Good resistance to SF6.Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.20 - 1.40 g/cc
1.20 - 1.40 g/cc
IEC 1212-2 8.1
Mechanical Properties Metric English Comments
Tensile Strength >= 135 MPa
>= 19600 psi
IEC 1212-2 5.7
Flexural Strength >= 110 MPa
>= 16000 psi
Perpendicular to laminations; IEC 1212-2 5.1
Compressive Strength >= 200 MPa
>= 29000 psi
Perpendicular to laminations; IEC 1212-2 5.3
Shear Strength >= 12.0 MPa
>= 1740 psi
Parallel to laminations; IEC 1212-2 5.6
Izod Impact, Unnotched (ISO) >= 145 kJ/m²
>= 69.0 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.3
Charpy Impact Unnotched >= 13.0 J/cm²
>= 61.9 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.2
Electrical Properties Metric English Comments
Insulation Resistance >= 1.00e+8 ohm
>= 1.00e+8 ohm
After immersion in water; IEC 1212-2 6.3
Dielectric Constant <= 5.3

@Frequency 48.0 - 62.0 Hz
<= 5.3

@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
<= 5.3

@Frequency 1.00e+6 Hz
<= 5.3

@Frequency 1.00e+6 Hz
IEC 1212-2 6.2
Dielectric Breakdown >= 55000 V

@Temperature 90.0 °C
>= 55000 V

@Temperature 194 °F
In oil, parallel to laminations; IEC 1212-2 6.2
Dissipation Factor <= 0.050

@Frequency 48.0 - 62.0 Hz
<= 0.050

@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
<= 0.050

@Frequency 1.00e+6 Hz
<= 0.050

@Frequency 1.00e+6 Hz
IEC 1212-2 6.2
Comparative Tracking Index >= 380 V
>= 380 V
IEC 1212-2 6.4
Descriptive Properties Value Comments
Thermal Endurance 130 T.I.
IEC 1212-2 7.1
Water Absorption < 220 mg
IEC 1212-2 8.2; Test piece 50 x 50 x 10 mm