Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hippe MF GC 21 Woven Glass Cloth Reinforced Melamine Resin - Round, Rolled Tube

Category Polymer , Thermoset , Melamine , Melamine Formaldehyde, Molded, Glass Fiber Filler
Manufacturer Erhard Hippe KG
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hippe MF GC 21 Woven Glass Cloth Reinforced Melamine Resin - Round, Rolled Tube.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used in mechanical and electrical applications. High mechanical strength. Good arc and tracking resistance. Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.70 - 1.90 g/cc
1.70 - 1.90 g/cc
IEC 1212-2 7.2
Mechanical Properties Metric English Comments
Flexural Strength >= 120 MPa

@Diameter >=100 mm
>= 17400 psi

@Diameter >=3.94 in
Perpendicular to laminations; IEC 1212-2 4.1
Compressive Strength >= 80.0 MPa
>= 11600 psi
Axial; IEC 1212-2 4.2
Electrical Properties Metric English Comments
Insulation Resistance >= 100000 ohm

@Diameter 8.00 - 10.0 mm
>= 100000 ohm

@Diameter 0.315 - 0.394 in
After immersion in water; IEC 1212-2 5.2
Dielectric Constant <= 8.0

@Frequency 1.00e+6 Hz
<= 8.0

@Frequency 1.00e+6 Hz
IEC 1212-2 5.3
Dielectric Breakdown >= 10000 V

@Temperature 90.0 °C,
Time 20.0 sec
>= 10000 V

@Temperature 194 °F,
Time 0.00556 hour
Step-by-step test, In oil, parallel to laminations; IEC 1212-2 5.1
>= 10000 V

@Temperature 90.0 °C,
Time 60.0 sec
>= 10000 V

@Temperature 194 °F,
Time 0.0167 hour
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1
Dissipation Factor <= 0.020

@Frequency 1.00e+6 Hz
<= 0.020

@Frequency 1.00e+6 Hz
IEC 1212-2 5.3
Descriptive Properties Value Comments
Cohesion between layers > 150 MPa
IEC 1212-2 4.3, Internal diameter <100 mm
Thermal Endurance 130 T.I.
IEC 1212-2 7.1
Water Absorption < 5 mg/cm²
IEC 1212-2 7.1