Material Notes:
Very tough, even at low temperatures. Hard. High attenuation properties. Technical components such as gear wheels, pinions, screws, nuts, bearings, seals, cloth components, guide components, pump components, armatures, housings, coils, etc.Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
DIN 53 479
Moisture Absorption at Equilibrium 1.6 - 2.0 %
1.6 - 2.0 %
Absorption of humidity in standard operating environment; DIN 53 715
Water Absorption at Saturation 6.5 - 7.5 %
6.5 - 7.5 %
DIN 53 495
Mechanical Properties Metric English Comments
Ball Indentation Hardness 190 MPa

@Time 30.0 sec
27600 psi

@Time 0.00833 hour
DIN 53 456
Tensile Strength 100 MPa
14500 psi
cond.; DIN 53 455
110 MPa
16000 psi
dry; DIN 53 455
Elongation at Break 10 %
10 %
dry; DIN 53 455
20 %
20 %
cond.; DIN 53 455
Tensile Modulus 3.50 GPa
508 ksi
DIN 53 457
Charpy Impact, Notched NB
NB
DIN 53 453
Coefficient of Friction, Dynamic 0.34 - 0.42
0.34 - 0.42
Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
Thermal Properties Metric English Comments
CTE, linear 55.0 µm/m-°C
30.6 µin/in-°F
Specific Heat Capacity 1.50 J/g-°C
0.359 BTU/lb-°F
Thermal Conductivity 0.230 W/m-K
1.60 BTU-in/hr-ft²-°F
Melting Point 295 °C
563 °F
DIN 53 736
Maximum Service Temperature, Air 100 °C
212 °F
Continuous use
180 °C
356 °F
Short Periods
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ISO-R 75 Method A
Flammability, UL94 V-2
V-2
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
DIN 53 482, VDE 0303, Part 3
Dielectric Constant 4.0

@Frequency 1.00e+6 Hz
4.0

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Dielectric Strength 50.0 - 80.0 kV/mm
1270 - 2030 kV/in
Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1
Dielectric Loss Index 0.030 - 0.040

@Frequency 1.00e+6 Hz
0.030 - 0.040

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Descriptive Properties Value Comments
Color natural/black
Creep Resistance Grade CTI 600
DIN 53 480, IEC-112, VDE 0303 Part 1
Resistance to hot water, suds resistant in some conditions