Hippe PAI Polyamide-imide

Category Polymer , Thermoplastic , Polyamide-imide (PAI)
Manufacturer Erhard Hippe KG
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hippe PAI Polyamide-imide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Particularly used where high strength in a wide range of temperature (-190°C…+260°C), high notched strength and very good dielectric properties are required. Features good chemical stability, flame resistance and high heat stability of shape.Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
DIN 53 479
Moisture Absorption at Equilibrium 2.5 %
2.5 %
Absorption of humidity in standard operating environment; DIN 53 715
Water Absorption at Saturation 3.5 %
3.5 %
DIN 53 495
Mechanical Properties Metric English Comments
Tensile Strength 192 MPa
27800 psi
DIN 53 455
Elongation at Break 15 %
15 %
DIN 53 455
Tensile Modulus 4.90 GPa
711 ksi
DIN 53 457
Flexural Modulus 5.00 GPa
725 ksi
from bending test; DIN 53 457
Coefficient of Friction, Dynamic 0.25 - 0.90
0.25 - 0.90
Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
Thermal Properties Metric English Comments
CTE, linear 31.0 µm/m-°C
17.2 µin/in-°F
Thermal Conductivity 0.260 W/m-K
1.80 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C
500 °F
Continuous use
260 °C
500 °F
Short Periods
Deflection Temperature at 0.46 MPa (66 psi) 278 °C
532 °F
ISO-R 75 Method B
Deflection Temperature at 1.8 MPa (264 psi) 275 °C
527 °F
ISO-R 75 Method A
Glass Transition Temp, Tg 275 °C
527 °F
dynamic; DIN 53 736
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+15 ohm-cm
2.00e+15 ohm-cm
DIN 53 482, VDE 0303, Part 3
Surface Resistance 5.00e+18 ohm
5.00e+18 ohm
DIN 53 482
Dielectric Constant 3.9

@Frequency 1.00e+6 Hz
3.9

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Dielectric Strength 23.6 kV/mm
599 kV/in
Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1
Dielectric Loss Index 0.031

@Frequency 1.00e+6 Hz
0.031

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Descriptive Properties Value Comments
Creep Resistance Grade CTI 600
DIN 53 480, IEC-112, VDE 0303 Part 1
Resistance to hot water, suds resistant in some conditions