Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hippe PEEK BG Polyetheretherketone with carbon fiber, PTFE and graphite

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Erhard Hippe KG
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hippe PEEK BG Polyetheretherketone with carbon fiber, PTFE and graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The addition to PEEK of carbon fiber, PTFE and graphite results in a material with high mechanical strength, a low coefficient of sliding friction and enhanced resistance to abrasion. The outstanding tribological properties of PEEK BG make it a particularly suitable material for friction bearing applications.Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
DIN 53 479
Water Absorption at Saturation 0.10 %
0.10 %
DIN 53 495
Mechanical Properties Metric English Comments
Elongation at Break 3.0 %
3.0 %
DIN 53 455
Tensile Modulus 10.0 GPa
1450 ksi
DIN 53 457
Flexural Modulus 8.10 GPa
1170 ksi
from bending test; DIN 53 457
Coefficient of Friction, Dynamic 0.11
0.11
Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
Tear Strength Test 118
118
in MPa; DIN 53 455
Thermal Properties Metric English Comments
CTE, linear 22.0 µm/m-°C
12.2 µin/in-°F
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
Melting Point 334 °C
633 °F
DIN 53 736
Maximum Service Temperature, Air 250 °C
482 °F
Continuous use
300 °C
572 °F
Short Periods
Deflection Temperature at 1.8 MPa (264 psi) 277 °C
531 °F
ISO-R 75 Method A
Glass Transition Temp, Tg 143 °C
289 °F
dynamic; DIN 53 736
Flammability, UL94 V-0
V-0
Descriptive Properties Value Comments
Color black
Resistance to hot water, suds resistant