Material Notes:
PEEK is a crystalline, easily machinable thermoplastic which is characterized by high tensile and constant good electrical properties between 0°-220°C, as well as due to favorable tribological behavior and flame resistance.Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
DIN 53 479
Moisture Absorption at Equilibrium 0.10 %
0.10 %
Absorption of humidity in standard operating environment; DIN 53 715
Water Absorption at Saturation 0.50 %
0.50 %
DIN 53 495
Mechanical Properties Metric English Comments
Tensile Strength 92.0 MPa
13300 psi
DIN 53 455
Elongation at Break 50 %
50 %
DIN 53 455
Tensile Modulus 3.60 GPa
522 ksi
DIN 53 457
Flexural Modulus 4.10 GPa
595 ksi
from bending test; DIN 53 457
Charpy Impact, Notched NB
NB
DIN 53 453
Coefficient of Friction, Dynamic 0.30 - 0.38
0.30 - 0.38
Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
Thermal Properties Metric English Comments
CTE, linear 47.0 µm/m-°C
26.1 µin/in-°F
Specific Heat Capacity 0.320 J/g-°C
0.0765 BTU/lb-°F
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
Melting Point 334 °C
633 °F
DIN 53 736
Maximum Service Temperature, Air 250 °C
482 °F
Continuous use
300 °C
572 °F
Short Periods
Deflection Temperature at 0.46 MPa (66 psi) 182 °C
360 °F
ISO-R 75 Method B
Deflection Temperature at 1.8 MPa (264 psi) 140 °C
284 °F
ISO-R 75 Method A
Glass Transition Temp, Tg 143 °C
289 °F
dynamic; DIN 53 736
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 4.90e+16 ohm-cm
4.90e+16 ohm-cm
DIN 53 482, VDE 0303, Part 3
Dielectric Constant 3.2 - 3.3

@Frequency 1.00e+6 Hz
3.2 - 3.3

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Dielectric Strength 20.0 kV/mm
508 kV/in
Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1
Dielectric Loss Index 0.0010 - 0.0040

@Frequency 1.00e+6 Hz
0.0010 - 0.0040

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Descriptive Properties Value Comments
Color gray
Creep Resistance Grade CTI 150
DIN 53 480, IEC-112, VDE 0303 Part 1
Resistance to hot water, suds resistant