Hippe POM Copolymer

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer Erhard Hippe KG
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hippe POM Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyacetals are particularly suitable for the manufacture of precision and technical components, bushing, spring elements, housing components, sliding elements, chains, curve discs, bearing, running, and fan wheels, bolts, pumps, toothed parts rollers, screws, valves, toothed wheels requiring dimensional accuracy.Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
DIN 53 479
Moisture Absorption at Equilibrium 0.30 %
0.30 %
Absorption of humidity in standard operating environment; DIN 53 715
Water Absorption at Saturation 0.50 %
0.50 %
DIN 53 495
Mechanical Properties Metric English Comments
Ball Indentation Hardness 155 MPa

@Time 30.0 sec
22500 psi

@Time 0.00833 hour
DIN 53 456
Tensile Strength 65.0 MPa
9430 psi
DIN 53 455
Elongation at Break 40 %
40 %
DIN 53 455
Tensile Modulus 3.10 GPa
450 ksi
DIN 53 457
Charpy Impact, Notched NB
NB
DIN 53 453
Coefficient of Friction, Dynamic 0.32
0.32
Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
Abrasion 8.9
8.9
µm/km; Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
Thermal Properties Metric English Comments
CTE, linear 100 µm/m-°C
55.6 µin/in-°F
Specific Heat Capacity 1.50 J/g-°C
0.359 BTU/lb-°F
Thermal Conductivity 0.310 W/m-K
2.15 BTU-in/hr-ft²-°F
Melting Point 165 °C
329 °F
DIN 53 736
Maximum Service Temperature, Air 100 °C
212 °F
Continuous use
140 °C
284 °F
Short Periods
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
ISO-R 75 Method B
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ISO-R 75 Method A
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
DIN 53 482, VDE 0303, Part 3
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
DIN 53 482
Dielectric Constant 3.5

@Frequency 1.00e+6 Hz
3.5

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Dielectric Strength >= 50.0 kV/mm
>= 1270 kV/in
Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1
Dielectric Loss Index 0.0030

@Frequency 1.00e+6 Hz
0.0030

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Descriptive Properties Value Comments
Color natural, black
Creep Resistance Grade CTI 600
DIN 53 480, IEC-112, VDE 0303 Part 1
Resistance to hot water, suds resistant in some conditions