Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Honeywell Capran® Emblem™ 2530 Bi-Axially Oriented Nylon Film  (discontinued **)

Category Polymer , Film , Thermoplastic , Nylon
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Honeywell Capran® Emblem™ 2530 Bi-Axially Oriented Nylon Film  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Capran® Emblem™ 2530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbons, and many solvents. It is also microwavable, making it an excellent choice for lidding stock.Applications: bag-on-box packaging, packaging for processed meats, cheese, meat snacks, coffee bricks, coffee bags, and pet food, agricultural bags, stand-up shampoo pouches, book covers and metallized balloons.Information provided by Honeywell.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0440 lb/in³
Yield Density
Water Vapor Transmission 9.31 - 12.42 g/m²/day
0.600 - 0.7998 g/100 in²/day
100°F / 100%RH); ASTM F1249
Oxygen Transmission Rate 7.76 - 13.97 cc/m²/day
0.500 - 0.8997 cc/100 in²/day
77°F / 0% / RH; ASTM D3985
Thickness 28.4 microns
1.12 mil
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 70 - 110 %
70 - 110 %
ASTM D882
Film Elongation at Break, TD 60 - 90 %
60 - 90 %
ASTM D882
Secant Modulus, MD 2.41 - 3.55 GPa
350 - 515 ksi
ASTM D882
Secant Modulus, TD 2.275 - 3.28 GPa
330.0 - 476 ksi
ASTM D882
Coefficient of Friction 0.21 - 0.41
0.21 - 0.41
film to stainless steel; ASTM D1894
0.65 - 0.86
0.65 - 0.86
film to film; ASTM D1894
Tear Strength Test 1150 - 1475
1150 - 1475
graves tear, grams/mil (initial); ASTM D1004
Elmendorf Tear Strength, MD 0.5272 - 0.6677 g/micron
13.39 - 16.96 g/mil
Film Tensile Strength at Break, MD 207 - 290 MPa
30000 - 42000 psi
ASTM D882
Film Tensile Strength at Break, TD 221 - 283 MPa
32000 - 41000 psi
ASTM D882
Thermal Properties Metric English Comments
Shrinkage, MD 1.6 - 2.3 %
1.6 - 2.3 %
320°F / 160°C - 5 minutes; ASTM D1204
Shrinkage, TD 0.20 - 0.70 %
0.20 - 0.70 %
320°F / 160°C - 5 minutes; ASTM D1204
Optical Properties Metric English Comments
Haze <= 5.0 %
<= 5.0 %
ASTM D1003
Gloss 75 - 85 %
75 - 85 %
at 20°
Copyright © lookpolymers.com All Rights Reserved