Huntsman AVALON® 650 B Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Huntsman Corporation
Trade Name Avalon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman AVALON® 650 B Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and translucencyOil resistanceFast cycle timesOutstanding abrasion and scratch resistancePerfect color match with masterbatchesRubber-like look and feelExcellent bonding.Information provided by Alliance Polymers
Physical Properties Metric English Comments
Density 0.650 g/cc
0.0235 lb/in³
ISO 2781
Mechanical Properties Metric English Comments
Hardness, Shore A 54
54
ISO 868
Tensile Strength at Break 5.00 MPa
725 psi
ISO 37
Elongation at Break 600 %
600 %
ISO 37
Flexural Modulus 0.0600 GPa
8.70 ksi
ISO 178
Tear Strength 17.0 kN/m
97.0 pli
ISO 34B
Abrasion 200
200
mm<sup>3</sup>; ISO 4649