Material Notes:
Weight per Epoxide (EEW, g/eq) 385 to 405. Max color is 3.Comments/Applications: Low viscosity, polypropylene glycol-based epoxy resin. Enhances flexibility and impact resistance.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 42 - 52 cP
42 - 52 cP