Huntsman Araldite EPN 1138 X-85 Epoxy Phenol Novolac

Category Polymer , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name Araldite
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Araldite EPN 1138 X-85 Epoxy Phenol Novolac.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Weight per Epoxide (EEW, g/eq) 176 to 181. Max color is 2.Comments/Applications: EPN 1138 75% solids in xylene. High performance, chemically resistant tank linings, maintenance coatings.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 3000 - 9000 cP
3000 - 9000 cP