Huntsman HT 939 Special Hardener

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman HT 939 Special Hardener.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mix Ratio with GY 6010 is 100 phr 35.Comments/Applications: Latent modified polyamide hardener. Excellent shelf life. Six month latency at RT. Excellent adhesion, good mechanicals, highly reactive at 100°C. Adhesives, tooling, vinyl plastisols, dipping compounds. Pale yellow powder.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Softening Point
Processing Properties Metric English Comments
Processing Temperature 150 °C
302 °F
Cure Schedule: 6.5 min @ 150°C