Material Notes:
Approx. H+ equivalent weight 130. Mix Ratio with GY 6010 is 81.Comments/Applications: Solvent free, low viscosity, high amine content with higher flexibility and toughness. Flexible mix ratio 33 - 100 PHR, with GY 6010. High solids or solvent free industrial coatings, adhesives, general purpose industrial.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 3000 - 6000 cP
3000 - 6000 cP
Processing Properties Metric English Comments
Pot Life 210 min
210 min