Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Huntsman IROGRAN® A 65 P 4324 N TPU-Polyether

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Huntsman Corporation
Trade Name IROGRAN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman IROGRAN® A 65 P 4324 N TPU-Polyether.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D995
Mechanical Properties Metric English Comments
Hardness, Shore A 71
71
ASTM D2240
Hardness, Shore D 22
22
ASTM D2240
Tensile Strength at Break 30.0 MPa
4350 psi
DIN 53504
Elongation at Break 900 %
900 %
ASTM D412
100% Modulus 0.00390 GPa
0.566 ksi
DIN 53504
300% Modulus 0.00980 GPa
1.42 ksi
DIN 53504
Rebound 58 %
58 %
Bayshore; ASTM D2632
Tear Strength 70.1 kN/m
400 pli
ASTM D624
Abrasion 60
60
[mm<sup>3</sup>]; ISO 4649
Compression Set 25 %

@Temperature 23.0 °C,
Time 252000 sec
25 %

@Temperature 73.4 °F,
Time 70.0 hour
ASTM D395
48 %

@Temperature 70.0 °C,
Time 86400 sec
48 %

@Temperature 158 °F,
Time 24.0 hour
ASTM D395
Thermal Properties Metric English Comments
Melting Point 110 - 164 °C
230 - 327 °F
Huntsman/TMA
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not reported
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved