Huntsman IROGRAN® A 85 P 5004 TPU-Polyether

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Huntsman Corporation
Trade Name IROGRAN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman IROGRAN® A 85 P 5004 TPU-Polyether.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
IROGRAN® A 85 P 5004 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications.Information provided by Alliance Polymers
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
injection molded; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
Injection molded; ASTM D2240
Hardness, Shore D 35
35
Injection molded; ASTM D2240
Tensile Strength at Break 12.4 MPa
1800 psi
25 mil film; ASTM D412
Elongation at Break 600 %
600 %
25 mil film; ASTM D412
100% Modulus 0.00689 GPa
1.00 ksi
25 mil film; ASTM D412
300% Modulus 0.00827 GPa
1.20 ksi
25 mil film; ASTM D412
Tear Strength 71.9 kN/m
410 pli
25 mil film; ASTM D624
Abrasion 140
140
mm<sup>3</sup>, injection molded; ISO 4649
Thermal Properties Metric English Comments
Melting Point 146 - 161 °C
295 - 322 °F
TMA Melt Range, 25 mil film
Flammability, UL94 V-0
V-0
Oxygen Index 34 %
34 %
injection molded; ASTM D2863