Information provided by Huntsman
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 94
94
Hardness, Shore D 46
46
Tensile Strength at Break 50.0 MPa
7250 psi
Elongation at Break 480 %
480 %
Tear Strength 95.0 kN/m
542 pli
Abrasion 35
35
[mm<sup>3</sup>]