Material Notes:
Introduction: IROGRAN CA116-205 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-205 is part of the HUNTSMAN film and sheet product range and offers a specially designed, flexible plasticizer free product suitable for the preparation of extruded films with enhanced adhesion following lamination. Performance Features: Low melt temperature High crystallization rate Good low temperature flexibility Good processability Applications: Adhesive film Lamination Information provided by Alliance Polymers
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Melt Index of Compound 60 g/10 min

@Load 5.00 kg,
Temperature 190 °C
60 g/10 min

@Load 11.0 lb,
Temperature 374 °F
MVR, [cm<sup>3</sup>/10 min]
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
Injection molded parts; ASTM D2240
Tensile Strength at Break 10.0 MPa
1450 psi
Injection molded parts; DIN 53504
Elongation at Break 600 %
600 %
Injection molded parts; DIN 53504
100% Modulus 0.00300 GPa
0.435 ksi
Injection molded parts; DIN 53504
300% Modulus 0.00400 GPa
0.580 ksi
Injection molded parts; DIN 53504
Tear Strength 80.6 kN/m
460 pli
Injection molded parts; ASTM D624
Thermal Properties Metric English Comments
Melting Point 80.0 - 110 °C
176 - 230 °F
TMA Melt Range
Processing Properties Metric English Comments
Feed Temperature 149 °C
300 °F
Extrusion
Middle Barrel Temperature 154 °C
309 °F
Extrusion
Adapter Temperature 154 °C
309 °F
Extrusion
Die Temperature 154 °C
309 °F
Extrusion