Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Huntsman KRYSTALFLEX® PE 399 Polyurethane Optical Aliphatic Film

Category Polymer , Film , Thermoplastic , Polyurethane, TP
Manufacturer Huntsman Corporation
Trade Name KRYSTALFLEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman KRYSTALFLEX® PE 399 Polyurethane Optical Aliphatic Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Tensile Strength at Break 44.8 MPa
6500 psi
ASTM D412
Elongation at Break 500 %
500 %
ASTM D412
100% Modulus 0.00207 GPa
0.300 ksi
ASTM D412
300% Modulus 0.00689 GPa
1.00 ksi
ASTM D412
Tear Strength 36.8 kN/m
210 pli
ASTM D624
Peel Strength 2.80 kN/m

@Temperature 85.0 °C
16.0 pli

@Temperature 185 °F
resistance to glass; ASTM D3167
11.7 kN/m

@Temperature 90.5 °C
67.0 pli

@Temperature 195 °F
resistance to glass; ASTM D3167
24.5 kN/m

@Temperature 99.0 °C
140 pli

@Temperature 210 °F
resistance to glass; ASTM D3167
24.5 kN/m

@Temperature 113 °C
140 pli

@Temperature 235 °F
resistance to glass; ASTM D3167
24.5 kN/m

@Temperature 118 °C
140 pli

@Temperature 244 °F
resistance to glass; ASTM D3167
24.5 kN/m

@Temperature 127 °C
140 pli

@Temperature 261 °F
resistance to glass; ASTM D3167
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -36.0 °C
-32.8 °F
Processing Properties Metric English Comments
Melt Temperature 80.0 - 140 °C
176 - 284 °F
Copyright © lookpolymers.com All Rights Reserved