Material Notes:
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ASTM D2240
Tensile Strength at Break 27.6 MPa
4000 psi
ASTM D412
Elongation at Break 440 %
440 %
ASTM D412
100% Modulus 0.00193 GPa
0.280 ksi
ASTM D412
300% Modulus 0.00827 GPa
1.20 ksi
ASTM D412
Tear Strength 28.9 kN/m
165 pli
ASTM D624
Peel Strength 14.0 kN/m

@Temperature 85.0 °C
80.0 pli

@Temperature 185 °F
resistance to glass; ASTM D3167
24.2 kN/m

@Temperature 90.5 °C
138 pli

@Temperature 195 °F
resistance to glass; ASTM D3167
24.2 kN/m

@Temperature 99.0 °C
138 pli

@Temperature 210 °F
resistance to glass; ASTM D3167
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -54.0 °C
-65.2 °F
Processing Properties Metric English Comments
Melt Temperature 65.0 - 125 °C
149 - 257 °F