Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Huntsman KRYSTALFLEX® PE 501 Polyurethane Optical Aliphatic Film

Category Polymer , Film , Thermoplastic , Polyurethane, TP
Manufacturer Huntsman Corporation
Trade Name KRYSTALFLEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman KRYSTALFLEX® PE 501 Polyurethane Optical Aliphatic Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Tensile Strength at Break 44.8 MPa
6500 psi
ASTM D412
Elongation at Break 350 %
350 %
ASTM D412
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D412
300% Modulus 0.00345 GPa
0.500 ksi
ASTM D412
Tear Strength 102 kN/m
580 pli
ASTM D624
Peel Strength 5.26 kN/m

@Temperature 91.0 °C
30.0 pli

@Temperature 196 °F
resistance to glass; ASTM D3167
19.6 kN/m

@Temperature 99.0 °C
112 pli

@Temperature 210 °F
resistance to glass; ASTM D3167
21.0 kN/m

@Temperature 113 °C
120 pli

@Temperature 235 °F
resistance to glass; ASTM D3167
22.3 kN/m

@Temperature 127 °C
127 pli

@Temperature 261 °F
resistance to glass; ASTM D3167
25.6 kN/m

@Temperature 118 °C
146 pli

@Temperature 244 °F
resistance to glass; ASTM D3167
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -31.0 °C
-23.8 °F
Processing Properties Metric English Comments
Melt Temperature 90.0 - 150 °C
194 - 302 °F
Copyright © lookpolymers.com All Rights Reserved