Material Notes:
Homopolymer and FDA compliant.Features: Good molding processability, produces parts that are flexible, and show excellent flatness in large projected areas.Applications: Injection molding: general purpose molding, housewares, and industrial parts.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)2.2 under condition of use B through H described in Table 2 of 21 CFR 176.170Information provided by Huntsman Corporation
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
ASTM D2240
Tensile Strength, Ultimate 10.0 MPa
1450 psi
ASTM D638
Tensile Strength, Yield 10.0 MPa
1450 psi
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Modulus of Elasticity 0.173 GPa
25.1 ksi
Secant; ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 86.0 °C
187 °F
ASTM D1525
Users viewing this material also viewed the following: